Aluminum Alloy 206
- The aluminum 206 alloy with the T7 temper meets the requirements for yield
strength (44 vs 40 ksi) and required elongation (11% vs 5%) , but fails to provide the
ultimate tensile strength (49 vs 50 ksi).
In addition, the alloy has poorer than desirable
weldability, machinability, corrosion resistance, and castability.
|